前言:挤出级PP,吹塑级PP,韩国sk,H870F,纤维级pp,汽车部件,塑胶原料
熔体流动速率 | 16 | g/10min | ASTM D-1238 |
IZOD缺口冲击强度 (23℃) | 3 | kg.cm/cm | ASTM D-256 |
表面硬度 | 104 | R scale | ASTM D-785 |
断裂拉伸强度 | 380 | Kg/cm | ASTM D-638 |
弹性弯曲系数 | 17000 | Kg/cm | ASTM D-790 |
断裂伸长率 | >500 | % | ASTM D-638 |
维卡软化点 | 155 | ℃ | ASTM D-1525 |
热变形温度 | 107 | ℃ | ASTM D-648 |
加速老化时间 | 360 | hr | ASTM D-3012 |
流动性 | >800 | mm | SK |