前言:PA6,德国巴斯夫,8202C,高流动,耐热,抗老化,耐高温,尼龙单6聚酰胺
物理性能额定值单位测试方法密度1.13g/cmISO 1183成型收缩率0.009in/inASTM D955吸水率 (24hrs)1.6%ASTM D570 (24h/23C)1.6%ISO 62 (73℉)9.3%ASTM D570 (23C)9.3%ISO 62 (23C/50RH)2.6%ISO 62吸湿率2.6%ISO 62硬度120ASTM D785机械性能额定值单位测试方法拉伸模量ISO 527-1,-2 (-40℉)593000psi (176℉)109000psi (248℉)79800psi537000psi拉伸屈服强度ASTM D638 (-40℉)19900psi (248℉)4350psi拉伸屈服应力ISO 527-1,-2 (-40℉)19900psi (176℉)5800psi (248℉)4350psi屈服应力12800psiISO 527-1,-2断裂拉伸强度ASTM D638 (-40℉)18900psi (176℉)5080psi (248℉)3630psi断裂拉伸应力 (-40℉)18900psiISO 527-1,-2屈服伸长率ASTM D638 (-40℉)3.0% (176℉)25% (248℉)27%屈服应变4.0%ISO 527-1,-2断裂伸长率ASTM D638 (-40℉)5.0% (176℉)**** (248℉)****弯曲模量ASTM D790 (-40℉)489000psi (73℉)460000psi (149℉)87000psi (199℉)63800psi (248℉)55800psi (73℉)406000psi弯曲强度ASTM D790 (-40℉)26500psi (73℉)16000psi (149℉)4350psi (248℉)3050psi (73℉)13800psiCHARPY缺口冲击强度 (23℃)1.67ft·lb/inISO 179/1eAIZOD缺口冲击ASTM D256 (-40℉)0.599ft·lb/in (73℉)0.899ft·lb/in电气性能额定值单位测试方法表面电阻系数>3.9E+12ohm·inIEC 60093热性能额定值单位测试方法熔点428℉阻燃性V-2ISO 1210企业新闻