基本性能额定值单位测试方法融体流动速率ASTM D-1238 (200℃/5kg)1g/10min (220℃/10kg)7g/10min熔体流动速率 (230℃/3.8kg)3g/10minASTM D-1238物理性能额定值单位测试方法比重1.08g/ccASTM D-792模具收缩率0.4-0.7%ASTM D-955机械性能额定值单位测试方法拉伸屈服强度 (50mm/min)450kg/cmASTM D-638拉伸模量 (1mm/min)23000kg/cmASTM D-638屈服伸长率 (50mm/min)6%ASTM D-638断裂伸长率 (50mm/min)20%ASTM D-638弯曲强度 (15mm/min)750kg/cmASTM D-790弯曲模量 (15mm/min)25500kg/cmASTM D-790IZOD缺口冲击强度ASTM D-256 (1/4" 23℃)18kg.cm/cm (1/4" -30℃)8kg.cm/cm (1/8" 23℃)19kg.cm/cm (1/8" -30℃)8kg.cm/cm洛氏硬度110R-scaleASTM D-785热性能额定值单位测试方法热变形温度ASTM D-648 (18.5kg/cm 1/4"退火)110℃ (18.5kg/cm 1/4"未退火)105℃ (4.6kg/cm1/4" 退火)119℃ (4.6kg/cm1/4" 未退火)114℃维卡软化点 (5kg, 50℃/h)115℃ASTM D-1525阻燃等级UL94 (1/8")HBcalss (1/16")HBcalss企业新闻