前言:PP,韩国SK,B380G,注塑级,高流动,高抗冲,高光泽,家电部件
熔体流动速率 | 25 | g/10min | ASTM D-1238 |
收缩率 | 1.5-2.0 | % | SK |
IZOD冲击强度 (-20℃) | 3 | kg.cm/cm | ASTM D-256 |
洛氏硬度 | 95 | R Scale | ASTM D-785 |
IZOD冲击强度 (23℃) | 8 | kg.cm/cm | ASTM D-256 |
断裂伸长率 | >300 | % | ASTM D-638 |
弯曲弹性系数 | 16000 | kg/cm | ASTM D-790 |
拉伸断裂强度 | 290 | kg/cm | ASTM D-638 |
加速老化时间 | 360 | hr | ASTM D-3012 |
热变形温度 | 110 | ℃ | ASTM D-648 |
维卡软化点 | 150 | ℃ | ASTM D-1525 |
流动性 | >800 | mm | SK |